Oil Drilling CMC
Slurry with CMC would form thin but hard filter cake with low permeability, reducing water loss. Adding CMC into slurry will endow the drill with low initial gel strength, making the slurry give off the gas inside and abandoning the waste into the slurry pit. Same as other suspending dispersion, the drill slurry has an existing period which will be stable and extended after adding CMC.
Slurry with CMC is seldom affected by the bacterium and requires no high PH value or corrosion resistant.Slurry with CMC has excellent stability and will still reduce the filtration loss under 150℃ or above.
CMC oilfield grade is divided into LV and HV.
1、Technical CMC LV
Models, quality indicators (meeting standard: GB/T 5005-2010 and API 13A)
Items | Specification |
Starch or its derivatives | Absent |
Viscometer 600r/min reading | ≤90 |
Fluids loss,ml | ≥10 |
2、Technical HV CMC
Models, quality indicators (meeting standard: GB/T 5005-2010 and API 13A)
Items | Specification |
Starch or its derivatives | Absent |
Viscometer 600r/min | IN DI H2O | ≥30 |
IN 40g/l NaCI | ≥30 |
IN SAT NacI | ≥30 |
Saturated salt water fluids loss,ml | ≤10 |